So lately i've been throwing a bunch of random stuff in my AR pot and my solutions have been coming out Dirty. Scrap cpu's, pins, ribbons, whatever i throw it in and i've gotten back a few dark Black pots.
1. I perform a stannous test, denox, chill, check my ph levels and drop with smb.
I then collect all my blacks sands and junk and boil it in 35% hcl until everythings gone.
I again perform #1. on my pregnant hcl solution.
Out comes the fluffy golden brown gold stuffs i'm used to seeing. I decant and clean with distilled h20.
Since i'm not familiar with dirty solutions what can i expect as far as gold purity without a double and triple refine. Is this 97% or 99% or .999.
1. I perform a stannous test, denox, chill, check my ph levels and drop with smb.
I then collect all my blacks sands and junk and boil it in 35% hcl until everythings gone.
I again perform #1. on my pregnant hcl solution.
Out comes the fluffy golden brown gold stuffs i'm used to seeing. I decant and clean with distilled h20.
Since i'm not familiar with dirty solutions what can i expect as far as gold purity without a double and triple refine. Is this 97% or 99% or .999.
Last edited: