C chrishawn Well-known member Joined Dec 1, 2009 Messages 84 Feb 17, 2010 #1 I have noticed vary small particals of gold in my filtered AP,what would be the best way to recover.
A Anonymous Guest Feb 17, 2010 #2 A finer filter would be my guess, or just keep using the ap over and over and eventually you will get them. Jim
A finer filter would be my guess, or just keep using the ap over and over and eventually you will get them. Jim
leavemealone Well-known member Joined Mar 19, 2009 Messages 576 Location Cocoa,FL Feb 17, 2010 #3 I have noticed vary small particals of gold in my filtered AP,what would be the best way to recover. Click to expand... **EDITED** Amazing how AP and AR look so close....lol. Decant,wash and dry.Test decanted solution for any gold before disposing. Johnny
I have noticed vary small particals of gold in my filtered AP,what would be the best way to recover. Click to expand... **EDITED** Amazing how AP and AR look so close....lol. Decant,wash and dry.Test decanted solution for any gold before disposing. Johnny
A aflacglobal Well-known member Joined Apr 27, 2007 Messages 1,511 Location ozone Feb 17, 2010 #4 Ap Ap Ap Ap Ap Ap Ap Ap Ap Ap Ap Ap !
C chrishawn Well-known member Joined Dec 1, 2009 Messages 84 Feb 17, 2010 #5 thanks, :x where would i get a refiner filter
leavemealone Well-known member Joined Mar 19, 2009 Messages 576 Location Cocoa,FL Feb 18, 2010 #6 Response edited. where would i get a refiner filter Click to expand... Finer filter. Johnny
samuel-a Well-known member Joined Oct 7, 2009 Messages 2,190 Feb 18, 2010 #7 chrishawn , just let settle for 24 hours, they will all be on the bottom
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida Feb 18, 2010 #8 A simple plastic funnel packed with a sheet or two of folded Charmin toilet tissue will remove all of the fine particles. The tissue plug can then be treated in AR or HCl-Cl directly to recover the gold. Steve
A simple plastic funnel packed with a sheet or two of folded Charmin toilet tissue will remove all of the fine particles. The tissue plug can then be treated in AR or HCl-Cl directly to recover the gold. Steve
A Anonymous Guest Mar 3, 2010 #9 stir and cook longer. I'm a newbie too, lol..tell me if it works.. it works for me.