L LEPPER New member Joined Aug 15, 2011 Messages 1 Aug 15, 2011 #1 HOW TO RECOVER THE COPPER IN THE COPPER NITRIC SOLUTION
Geo Well-known member Joined Mar 1, 2011 Messages 7,069 Location Decatur,Ala. Aug 15, 2011 #2 after all other values have been extracted, just place a piece of clean steel in the solution and the copper will cement out into powder in the bottom of your container.
after all other values have been extracted, just place a piece of clean steel in the solution and the copper will cement out into powder in the bottom of your container.
Harold_V Well-known member Moderator Emeritus Joined Feb 25, 2007 Messages 8,360 Aug 15, 2011 #3 LEPPER said: HOW TO RECOVER THE COPPER IN THE COPPER NITRIC SOLUTION Click to expand... Use scrap steel, as has been advised. Please do not post in all caps. Use them only appropriately. Harold