i have dust containing gold and metals how can i refine pure gold
sakosakarian said:i have dust containing gold and metals how can i refine pure gold
sakosakarian said:there are factories that collect dust on the ground that would be full of metals, soil, dust, metals,... so what im doing is burning them then magnetizing to take out the metals, afterwards i apply aqua regia, then i put caustic soda to kill to acid then i filter and then sodium sulfite is added. gold drops to the bottom and calcareous substance as well as impurities also deposits with it. how can i improve my method so that no impurities are obtained with the gold in the end?