frank-20011
Well-known member
- Joined
- Jul 18, 2015
- Messages
- 183
Hello,
i've looked these video:
https://www.youtube.com/watch?v=BxU2n6BibE4
and between 9:14 and 9:40 you can see how cody melts an alloy of Ag-Pb an a fragment of ? (i don't understand the word) and thru this the shard absorbs the molten lead and left behind the gold.
What a material is the shard made of, are here in the forum any threads about these kind to work and works it with other metals like tin?
Regards, Frank!
i've looked these video:
https://www.youtube.com/watch?v=BxU2n6BibE4
and between 9:14 and 9:40 you can see how cody melts an alloy of Ag-Pb an a fragment of ? (i don't understand the word) and thru this the shard absorbs the molten lead and left behind the gold.
What a material is the shard made of, are here in the forum any threads about these kind to work and works it with other metals like tin?
Regards, Frank!