L Lou Moderator Staff member Moderator Joined Nov 4, 2007 Messages 5,237 Location Rhodia Drive Sep 26, 2013 #21 Sonication does indeed work for digesting karat.
C chlaurite Well-known member Joined Mar 17, 2013 Messages 209 Sep 27, 2013 #22 Lou said: Sonication does indeed work for digesting karat. Click to expand... So, that then leaves us with one slight problem for trying this out... Anyone know of a relatively cheap ultrasonic bath made of acid-resistant plastic?
Lou said: Sonication does indeed work for digesting karat. Click to expand... So, that then leaves us with one slight problem for trying this out... Anyone know of a relatively cheap ultrasonic bath made of acid-resistant plastic?
g_axelsson Administrator Staff member Administrator Moderator Joined Nov 17, 2007 Messages 5,536 Location Sweden Sep 27, 2013 #23 Test with a glass beaker inside the ultrasonic tank. Göran