i have 7 from this think is from Russia
did anybody knows how much gold in it
and how to process
thanks
 

Attachments

  • RussiaK573RF5_2.jpg
    RussiaK573RF5_2.jpg
    44.9 KB
There's not enough gold in it to surpass it's value
to chip collectors. :shock:

It would be worth your time to investigate their resale
value before you dunk them in nitric.
 
Руку шы еру сршз ензу шт снкшддшс

whoops, wrong keyboard

Here is the chip type in Cyrillic in case you want to search on it

к573рф5

Eprom.

"сделано в ссср" is "Made in USSR"
 
39mg Au or 1% Au from total mass(weight)
...also 49mg Ag or 1,4%