Trinity Gold videos is what end up bringing me to this forum. And now that I start reading hokes book, reading on this forum for the past few months, I'm proudly getting good clean gold every time. Still in small amounts as I'm doing small experiments. But with a fraction of the chemicals that are suggested in his videos. Which in the end means less waste to process safely
Congratulations on being able to retrieve good clean gold it isn’t easy to do. Keep up the good work brother, isn’t it such a cool and intriguing also very dangerous process.
 
Congratulations on being able to retrieve good clean gold it isn’t easy to do. Keep up the good work brother, isn’t it such a cool and intriguing also very dangerous process.
Yes it is very very cool. But unlike making fireworks there's a little money on the end instead of going up and smoke. I've still got one jar and one bucket of junk from my first attempt of recovery. Here soon I'll make a tread on it with a plan to get it right. If some of the other guys have some inside advice on it but that would be a little bit later on. Happy prospecting my friend!
 
Ok sorry for going MIA for a couple days, went to go see some family….So ygg I did as you said boiled it all down until it solidified this is what I got from that, I did preform a Stan out test while still liquid it was positive. Now I’m about to incinerate what’s left then dissolve in HCL image.jpg
 
Ok sorry for going MIA for a couple days, went to go see some family….So ygg I did as you said boiled it all down until it solidified this is what I got from that, I did preform a Stan out test while still liquid it was positive. Now I’m about to incinerate what’s left then dissolve in HCL View attachment 66402
I'm a bit confused, which of my advice called you to boil it dry?
Very strange color anyway.
And it is Stannous, not "Stan out" I'm not sure where that come from.
 
I'm a bit confused, which of my advice called you to boil it dry?
Very strange color anyway.
And it is Stannous, not "Stan out" I'm not sure where that come from.
I’m sorry for choice of words used. I filtered the metastanic acid the dried it so I could roat it then dissolve in Hcl, I meant stannous my iPhone auto corrected I apologize IMG_3705.png
I must have misunderstood I took that as to take the moisture out and then roast it with my torch
 
I’m sorry for choice of words used. I filtered the metastanic acid the dried it so I could roat it then dissolve in Hcl, I meant stannous my iPhone auto corrected I apologize View attachment 66403
I must have misunderstood I took that as to take the moisture out and then roast it with my torch
Roast ughh sometimes I hate this stupid phone
 
I’m sorry for choice of words used. I filtered the metastanic acid the dried it so I could roat it then dissolve in Hcl, I meant stannous my iPhone auto corrected I apologize View attachment 66403
I must have misunderstood I took that as to take the moisture out and then roast it with my torch
Yes the Metastannic acid will need to be dried.
It will become a dry powdery substance.
Then you heat it to a low dull read while stirring.
It will still be a powder if I understand it correctly.
When this is done you dissolve it in HCl.
Any Gold foils or powder will be left as solids in the bottom.
 
Yes the Metastannic acid will need to be dried.
It will become a dry powdery substance.
Then you heat it to a low dull read while stirring.
It will still be a powder if I understand it correctly.
When this is done you dissolve it in HCl.
Any Gold foils or powder will be left as solids in the bottom.
Wow boy did I screw the proverbial pooch on that one, I took the sludge and then burnt it, then roasted it wow 🤯.
 