No, this is the metallic silver that was poured out of the crucible into cold water, this is the melted silver that was in the crucible that contained both melted silver and the unmelted crumbled pieces. The crumbled pieces (which contain small pieces of melted silver buttons) was taken out of the crucible and placed on the left of the graphite mold in the corningware, while the melted silver was poured into cold water. To add clarity, the pictures do not contain any silver chloride prior to the lye/sugar conversion, everything in the pics is after the lye/sugar conversion. I probably should have stated this beforehand.