SilverMac18
Member
- Joined
- Jan 25, 2020
- Messages
- 6
So I have searched everywhere on this topic. On here and on the web. Can not find the answer to this. I’ve been using distilled water from Walmart. The same brand every time and have had no issues. Until now. Every time I make my electrolyte for the cell the liquid is clear. Then I add the distilled water and it clouds up so bad I can’t see the bottom of the cell. Is this just bad water. Should I have it tested for chlorine? I’m at a loss and scratching my head. I’ve even tried filtering the solution and it will not filter out clear. Can I still use this for my cell or is it ruined? Any suggestions or help would be greatly appreciated. As I’m at a loss on what to do.