HI, did the clorine peroxide to 600 grams of cut ram fingers. after the smb drop it dried for a couple of months in the mason jar. I noticed some crystals small white in there. They are square. Wondering what they are. Tim
 
I assume you are referring to HCl /Cl or acid /peroxide? FYI, use correct terminology for everyone's sake. on that note, ore is smelted, gold is melted.
that being said, square crystals usually mean halides to me- salt, sodium chloride left over from the reaction
 
NaCl crystals is sqare and white. so, yea table salt, just dont put any on your eggs. :shock: :lol:
 