Bc I was was wondering if I could just skip the whole pre-process my material thing, save time and money on acids, and just dissolve it all at once and use Soah to precipitate out the iron, which I found out that I can, and I was wondering what my ph limits were by doing this... I work with Gold (III) oxide and iron, so the gold dissolves in hcl alone without an oxidizer. So no matter what I do, if I try cleaning material with pre-acid treatment, gold will still go into solution... which really complicates things for me... And because of the high iron content, the gold has hard time falling out. I'd first have to roast the material, converting back into metallic gold, and THEN pretreat it with acid to remove base metals. But anyways this response is getting way too long. Gotta roll.
As long as the Gold is dissolved just use one of the usual precipitants.
It won't touch the Iron.
Make sure the pH is no higher than 2 and then add SodiumMetaBisulfite (SMB) or Ferrous Sulfate.
The Gold should drop straight out with the Iron still in solution.
 
As long as the Gold is dissolved just use one of the usual precipitants.
It won't touch the Iron.
Make sure the pH is no higher than 2 and then add SodiumMetaBisulfite (SMB) or Ferrous Sulfate.
The Gold should drop straight out with the Iron still in solution.
Mine won't drop bc of the super super high iron content. Also ph of 3 to 3.5 would probably make larger particles. Iron, particularly in its Fe³⁺ (ferric) form, can also be reduced by sodium metabisulfite, potentially competing with gold (Au³⁺) for reduction. This is a problem for me. But we'll try adjusting the ph, and see if it works. Appreciate the advice.
 
Mine won't drop bc of the super super high iron content. Also ph of 3 to 3.5 would probably make larger particles. Iron, particularly in its Fe³⁺ (ferric) form, can also be reduced by sodium metabisulfite, potentially competing with gold (Au³⁺) for reduction. This is a problem for me. But we'll try adjusting the ph, and see if it works. Appreciate the advice.
I usually precipitate at 0-1 pH, The 2-4 boundary is closer to where it will not drop anymore.
If you have trouble try to cement it on Copper.
It will drop precious metals only and Mercury if it is there.
 
At what ph does gold precipitate from solutions? I have looked at hokes book, scoured for days online, looked at patents and can't find anything. I found a list of metals that precipitate by PH but platinum and gold weren't on it... You said by reactivity series... So this means gold would be one of the last to fall out? Appreciate any response.
Theoretically it should be the first to come out (after platinum). Metal nobility is an expression of how little energy is needed to reduce them. Not sure if that works in practice.

If you have iron and gold in solution and want to isolate the gold, why not cement on solid copper?
 
Strange, but ferrous sulfate (copperas) is the ideal precipitant as it will not reduce iron in solution to the metallic state as SMB will because of SO2.
 
Theoretically it should be the first to come out (after platinum). Metal nobility is an expression of how little energy is needed to reduce them. Not sure if that works in practice.

If you have iron and gold in solution and want to isolate the gold, why not cement on solid copper?
Because I want it to drop as a beautiful golden orange powder hahaha, if it doesn't drop I just throw the dissolved gold away and try again, lol.
 
I somewhat agree that these posts are unprofessional. I have 70,000 SIM cards I had XRF tested to type 1SIM 8.9 AU% and type2 4,4% AU content, Ni & CU being the Main elements tested.
AU content and base metals should be determined first and yields via processing then examined for maximum effective refinement.
All acids used should be content listed to avoid confusion.
The references to Hock's outdated book quoting 50c utensils should've been rewritten by any true Gold enthusiast on this site.
I don't intend at all to criticize this site & appreciate the dedication by the members, but am finding it also unhelpful. I would've gladly paid for proper advice but now believe I have to try elsewhere.
 
I somewhat agree that these posts are unprofessional. I have 70,000 SIM cards I had XRF tested to type 1SIM 8.9 AU% and type2 4,4% AU content, Ni & CU being the Main elements tested.
AU content and base metals should be determined first and yields via processing then examined for maximum effective refinement.
All acids used should be content listed to avoid confusion.
The references to Hock's outdated book quoting 50c utensils should've been rewritten by any true Gold enthusiast on this site.
I don't intend at all to criticize this site & appreciate the dedication by the members, but am finding it also unhelpful. I would've gladly paid for proper advice but now believe I have to try elsewhere.
This post did not help either.
Completely off topic.

Since you are into professionalism, please reread your own post with regard to names and chemical naming conventions.
I find it slightly humorous.
 
By the way, a rewrite of Hocks Hoke's book as referred to as the bible could have step by step flow charts. As an electronics technician who uses service manuals, checking voltages to isolate and streamline procedure is valuable. Again, determine AU Au and metals content first to determine yield percentage to make recovery a science instead of a recipe.

Edited by moderator to correct errors
 
Last edited by a moderator:
By the way, a rewrite of Hocks Hoke's book as referred to as the bible could have step by step flow charts. As an electronics technician who uses service manuals, checking voltages to isolate and streamline procedure is valuable. Again, determine AU Au and metals content first to determine yield percentage to make recovery a science instead of a recipe.

Edited by moderator to correct errors
This has been covered earlier.
One do not rewrite books unless one have some kind of consent from the owners of said property.
Next flow charts are only possible in the constraint of that all factors are known.
In refining there are simply too many unknown factors, so one really just need to learn the chemistry.

Within a refinery one can and have, I guess flow charts but a refinery usually deal with a defined set of feed-stock.
 
Theoretically it should be the first to come out (after platinum). Metal nobility is an expression of how little energy is needed to reduce them. Not sure if that works in practice.

If you have iron and gold in solution and want to isolate the gold, why not cement on solid copper?
Well, with hydroxide you're NOT reducing the metal. You're mostly changing the salting anion. Some metals will OXIDIZE further, not reduce, because sodium hydroxide is an oxidizing agent. And what will drop out then depends ENTIRELY upon that hydroxide (or oxide's) solubility in the solution.
 
I somewhat agree that these posts are unprofessional. I have 70,000 SIM cards I had XRF tested to type 1SIM 8.9 AU% and type2 4,4% AU content, Ni & CU being the Main elements tested.
AU content and base metals should be determined first and yields via processing then examined for maximum effective refinement.
All acids used should be content listed to avoid confusion.
The references to Hock's outdated book quoting 50c utensils should've been rewritten by any true Gold enthusiast on this site.
I don't intend at all to criticize this site & appreciate the dedication by the members, but am finding it also unhelpful. I would've gladly paid for proper advice but now believe I have to try elsewhere.
Chemistry doesn't change with time. The chemicals used in these processes today work in EXACTLY the same way they did decades ago. The only changes have come from processing more complicated metals like PGMs, where new compounds and more intricate methods of extracting them have been discovered. But that's because they were never easy to process and purify in the first place.

Palladium, for instance, wasn't even discovered until 1802, so it's not unusual for a new method to still pop up involving its recovery and purification. Gold, however, has been processed by humans for THOUSANDS of years, with entire nations bent upon getting every speck of it they could find. The methods for its chemical and thermal processing have been EXHAUSTIVELY studied by huge industries.

If the big-timers are using a particular method, it's almost certainly because it works better than other methods. As far as I can find, NO ONE in the industry recovers gold using sodium hydroxide to drop gold salts. That's a pretty good indicator it's not a useful method.
 
Well, with hydroxide you're NOT reducing the metal. You're mostly changing the salting anion. Some metals will OXIDIZE further, not reduce, because sodium hydroxide is an oxidizing agent. And what will drop out then depends ENTIRELY upon that hydroxide (or oxide's) solubility in the solution.
You're right. It should not depend on reduction potential. I was not thinking clearly.
 
Chemistry doesn't change with time. The chemicals used in these processes today work in EXACTLY the same way they did decades ago. The only changes have come from processing more complicated metals like PGMs, where new compounds and more intricate methods of extracting them have been discovered. But that's because they were never easy to process and purify in the first place.

Palladium, for instance, wasn't even discovered until 1802, so it's not unusual for a new method to still pop up involving its recovery and purification. Gold, however, has been processed by humans for THOUSANDS of years, with entire nations bent upon getting every speck of it they could find. The methods for its chemical and thermal processing have been EXHAUSTIVELY studied by huge industries.

If the big-timers are using a particular method, it's almost certainly because it works better than other methods. As far as I can find, NO ONE in the industry recovers gold using sodium hydroxide to drop gold salts. That's a pretty good indicator it's not a useful method.
Thankyou. And while processing Gold has existed for millennia we now have reverse electroplating techniques and simple preliminary XRF testing to determine AU content.
While Hoke's book a compendium a rewrite in format and technique as in "for dummies" series format an idea for any more experienced gold blog member to consider perhaps.

Much of the confusion I feel in first not determining E waste content via XRF or other first to determine yield by process, lack of general saturation guidelines of solutions as a few variables, as is size of product for processing (ie: I'll attempt to shred my Type2 SIMS to expose the plating behind epoxy). Other variables in aeration and heat, chemical strengths etc can be plotted via graph to obtain effects of time and material penetration.

I may run an experiment in dissolving CU and NI in solution first to determine effective methods of base metal targeting. Even a simple flow chart of "Stannous test solution None YES, NO proceed next step or repeat advances AU recovery from being a bakers recipe to CNC engineering.
 
Thankyou. And while processing Gold has existed for millennia we now have reverse electroplating techniques and simple preliminary XRF testing to determine AU content.
While Hoke's book a compendium a rewrite in format and technique as in "for dummies" series format an idea for any more experienced gold blog member to consider perhaps.

Much of the confusion I feel in first not determining E waste content via XRF or other first to determine yield by process, lack of general saturation guidelines of solutions as a few variables, as is size of product for processing (ie: I'll attempt to shred my Type2 SIMS to expose the plating behind epoxy). Other variables in aeration and heat, chemical strengths etc can be plotted via graph to obtain effects of time and material penetration.

I may run an experiment in dissolving CU and NI in solution first to determine effective methods of base metal targeting. Even a simple flow chart of "Stannous test solution None YES, NO proceed next step or repeat advances AU recovery from being a bakers recipe to CNC engineering.
Are there a particular reason why you write the elements in upper case?
In chemistry it is always upper case for the first letter and if there are a second it is in lower case.
Example KI is Potassium Iodine
AU don't exist since ther are no element with a single A.
 
While Hoke's book a compendium a rewrite in format and technique as in "for dummies" series format an idea for any more experienced gold blog member to consider perhaps.
No. Simply because hydrometallurgy is not for dummies. You need to study and get experience.
And as Yggdrasil said, there is no 'one size fits all' manual.
You would have 1000 manuals which are very similar at first glance. How would a dummy choose the right one?