i make many tests a day with stanous chloride in a spot plate for gold and palladium----then i add these tests in a becker with some water and ar---this becker contains gold and pd .How can i precipitate the gold and pd from this becker?
 
Precipitate the solution with zinc or copper, incinerate the resulting powder to red heat (do not melt!!), treat the powder with hot 35% HNO3 to extract the Pd, and finally dissolve the gold in AR.