Here's some pics of stannous chloride reaction from SSN initial Color goes brown then pink then stays orangish for a long time Assays are saying gold highest then traces of pgms. I get alot of precip from Leach but not having any luck converting to metal. Anyone recognize these colors. Maybe assays weren't accurate and I'm dealing with pgms rather than gold. Not sure. Any help would be great.its not letting me upload the first pic,