A Anonymous Guest Aug 4, 2010 #1 From a batch of chips, the liquor tested with stannous a nice green then changed to a lime green. Any ideas! Palladium and ?.
From a batch of chips, the liquor tested with stannous a nice green then changed to a lime green. Any ideas! Palladium and ?.
lazersteve Well-known member Joined Feb 27, 2007 Messages 7,334 Location Florida Aug 4, 2010 #2 Gus, Where is the test spot on the paper? Pd is best tested for with DMG, especially when testing a mixed metal solution. Pd with stannous will start out orange and turn green depending on concentration. Positive Pd stannous tests also tend to fade overnight. Steve
Gus, Where is the test spot on the paper? Pd is best tested for with DMG, especially when testing a mixed metal solution. Pd with stannous will start out orange and turn green depending on concentration. Positive Pd stannous tests also tend to fade overnight. Steve