mda20 Well-known member Joined Oct 7, 2011 Messages 92 Nov 14, 2011 #1 Hi Everybody. I met a man has some stones he said: " They contain silver'. How can I test those stones? Is it benefit to recover silver from them? Regards, MDA20
Hi Everybody. I met a man has some stones he said: " They contain silver'. How can I test those stones? Is it benefit to recover silver from them? Regards, MDA20
N nickvc Moderator Staff member Moderator Joined Sep 14, 2009 Messages 5,621 Location birmingham Nov 14, 2011 #2 Assay. From what I understand very little silver is recovered as metallics or in a very pure form so I can't see another way to get an answer that would be reliable.
Assay. From what I understand very little silver is recovered as metallics or in a very pure form so I can't see another way to get an answer that would be reliable.