I posted the other day about gold stripper cell and got great help, thanks again. The rinse water is an emerald green.
Is this normal or do I have base metals in the sulfuric acid?
If I do will I need to drop the metals?
Before or after re-concentrating the acid?
What will I need to use to drop the base metals?
Thanks in advance for the help.
Mark
Is this normal or do I have base metals in the sulfuric acid?
If I do will I need to drop the metals?
Before or after re-concentrating the acid?
What will I need to use to drop the base metals?
Thanks in advance for the help.
Mark