Here are some of my detector finds from this past summer. Cold weather is upon me here in Nevada and time to think about next year, maybe process some scrap and a few other tasks. Still it was a good year prospecting and this is only a part of my finds......
The three largest nuggets at the top are (from left to right) 0.52 ounces, 1.1 ounces and 0.41 ounces.