This is from a batch of gold filled. Dilute nitric, AR. It was Super fine, washing/filtering issues so I did AR again, water wash. Used SMB both times.
Read about sulfuric wash helping it clump and the photo is the decanted sulfuric.
The second photo is after water wash, with what did clump and drying. Still has a lot of super fine powder.
Any thoughts why this is so fine, it passes right through filters.
After the super fine from the water & sulfuric wash settle Anything else I should try?
I'll try it through another round of AR/smb.
Read about sulfuric wash helping it clump and the photo is the decanted sulfuric.
The second photo is after water wash, with what did clump and drying. Still has a lot of super fine powder.
Any thoughts why this is so fine, it passes right through filters.
After the super fine from the water & sulfuric wash settle Anything else I should try?
I'll try it through another round of AR/smb.