Hi everybody,

Coming back to society, I just got my pure tin granular from my brother who came back from Penang, Malaysia.

So, anyway, many thanks for all the suggestion and idea. It is all excellent.

Thank you very much
 
I went to a plating shop they gave me a tin ingot.
I cleaned it and melted
mixed some hcl/SnCL2/d.water

Melted 1 of 16 pounds of 62% tin solder

Put the solder bar on the + terminal of my rectifier
- on my tin bar

set it at 5v @ 10 amps in a small container.

The lead and silver are at the bottom and the tin side is 284g heavier.
 