V vivalalynn Member Joined Nov 5, 2012 Messages 10 Nov 10, 2012 #1 hello all, could somebody tell me is it possible to use too much stump out? if you can and do, how do you fix that problem? thank you all
hello all, could somebody tell me is it possible to use too much stump out? if you can and do, how do you fix that problem? thank you all
Geo Well-known member Joined Mar 1, 2011 Messages 7,069 Location Decatur,Ala. Nov 10, 2012 #2 warm the solution to steaming and keep it there until the solution clears.
J jimdoc Well-known member Joined Mar 12, 2007 Messages 4,943 Location Philadelphia Nov 10, 2012 #3 You have to make sure you are using the right stumpout. If it isn't working it may be the wrong type. Jim
You have to make sure you are using the right stumpout. If it isn't working it may be the wrong type. Jim
S steyr223 Well-known member Joined Oct 9, 2011 Messages 930 Location Fullerton ,California. usa Nov 11, 2012 #5 Make sure it's from home depot. It has I think a blue (maybe purple) cap and a square white plastic container. I believe its bodine "I think I'm spelling that wrong." Lows brand is potassium nitrate Look for my new post right here as it will Be close to the same subject it may help Thanks Steyr223 rob
Make sure it's from home depot. It has I think a blue (maybe purple) cap and a square white plastic container. I believe its bodine "I think I'm spelling that wrong." Lows brand is potassium nitrate Look for my new post right here as it will Be close to the same subject it may help Thanks Steyr223 rob
T tek4g63 Well-known member Joined Nov 4, 2011 Messages 406 Location Tennessee Nov 11, 2012 #6 I believe its " Bondie" Stump Out.
Geo Well-known member Joined Mar 1, 2011 Messages 7,069 Location Decatur,Ala. Nov 11, 2012 #7 actually, its Bonide. but its all good. when i was in the military, i answered to moosey,mossey,macey,messey, you get it. :lol:
actually, its Bonide. but its all good. when i was in the military, i answered to moosey,mossey,macey,messey, you get it. :lol: