I was given these molten blobs which where gold plated, bronze barreled pogo pins and gold plated, brass pins.
Total weight was a little over 9oz. I was able to disolve base metals and isolate the gold, then refine twice to get this tiny button. Its tiny but very high quality and my best one so far.
 