I was given these molten blobs which where gold plated, bronze barreled pogo pins and gold plated, brass pins.
Total weight was a little over 9oz. I was able to disolve base metals and isolate the gold, then refine twice to get this tiny button. Its tiny but very high quality and my best one so far.
Total weight was a little over 9oz. I was able to disolve base metals and isolate the gold, then refine twice to get this tiny button. Its tiny but very high quality and my best one so far.