Yeah, so what’s the point of your comment? We’re discussing doing it incorrectly in order to save time so the answer is is “yes, AP can risk dissolving gold if there is an excessive amount of tin remaining on the fingers prior to treatment with AP as the tin can cause colloidal gold to form”Nope. AP wont dissolve any gold if done correctly.