Using peracetic acid (Vinegar 5% & H2O2 3%) electrolyte to strip a silverplate dish. The solution came from the other silverplate stripping, that was used after electrolysis to get the slimes into solution. Turns out copper acetate is percipitating the copper as the reaction occurs. I have to keep scraping the cathode off for, the copper in the solution is percipitating on it.1000005006.jpg
 
The blue color is copper in solution. Electrolysis will electrowin it out on the cathode, and if reactivity permits it will cement(precipitate) out on any more rective metal when electricity is off.
After reading about it, try tap water. And a silver plated anode and cathode.

You made a copper cementing vinegar battery. Not a silver stripping cell.
Which is great to learn how to 'deal with waste'.

Study and read a lot, ask and present your plan before you go and copy another youtube 'tutorial' please.
 