I made a nitric solution,put in this solutio 440grams of the thick pins.Imediately i obtained the gold foils--i filtered the foils out,and put it in ar to obtain the gold---to the nitric solution i added Hcl,imediatelly formed silver choride--The pins was gold and silver,not berilyum bronze-tomorow i will test for palladium(the nitric solution) and see how many grams of gold and silver was obtained from 440grams of pins--Regards to all Arthur
 
I bought 200 pounds of scrap canon plugs and found that the yield varies on the diameter of the pins. Usually around 0.75% to 1.75% on the thinner pins. The thickness of the the silver under the gold is about the same thickness as the gold. The silver yields 1-2 grams per pound with the highly controversial hot sulfuric 80C and nitric acid method. BTW do not try the silver stripping solution, it is very dangerous and needs proper PPE and ventilation. As said many times on this forum do not attempt
 

Latest posts

Back
Top