S spoke27 Well-known member Joined Aug 22, 2008 Messages 119 Location Turkey Oct 8, 2008 #1 I have some question? What is best method for part gold on the Cpu? can I use ammonium nitrate +Hcl ? Or must be use sodium nitrate ?
I have some question? What is best method for part gold on the Cpu? can I use ammonium nitrate +Hcl ? Or must be use sodium nitrate ?
JustinNH Well-known member Joined Mar 16, 2008 Messages 259 Location New Hampshire Oct 8, 2008 #2 I suggest you read through the forum, use the search function as well. Different ways to do it are all discussed in great detail.. what to do and what not to do. Everything you need to know is here somewhere, welcome to the forum
I suggest you read through the forum, use the search function as well. Different ways to do it are all discussed in great detail.. what to do and what not to do. Everything you need to know is here somewhere, welcome to the forum
L Lino1406 Well-known member Joined Nov 1, 2007 Messages 2,356 Location Israel Oct 11, 2008 #3 You can use ammonium nitrate. But.. I suggest only on small scale and be sure to dispose off any remnants
You can use ammonium nitrate. But.. I suggest only on small scale and be sure to dispose off any remnants