What is the sensitivity of SnCl2 test for Au, Pt and Pt?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
well i have read 4 ppm for gold. But I think you could test just about any solution. evaporate the sample down then read. but its a judgement, anyways.

Jim
 