So I just dropped about 25 g of gold and I'm testing the solution after the Gold has been dropped and settled and the stannous chloride test shows this. What's this color mean? If it's platinum. Will it may be beyond my areas of experience.
Nevermind I tested it and it was simply gold that somehow made a film of sorts. So I just redissolved it.I also found this in my gold powder when washing it it looks like paper but coated in gold. I'm 99% certain that there was nothing in there when doing this procedure that looks like this. There wasn't anything in there. I have it now sitting in Hcl.
False positive, due to the excess SMBSo I just dropped about 25 g of gold and I'm testing the solution after the Gold has been dropped and settled and the stannous chloride test shows this. What's this color mean? If it's platinum. Will it may be beyond my areas of experience.