Northern California
So I just dropped about 25 g of gold and I'm testing the solution after the Gold has been dropped and settled and the stannous chloride test shows this. What's this color mean? If it's platinum. Will it may be beyond my areas of experience.
 

Attachments

  • 16644029490958989812375402000228.jpg
    16644029490958989812375402000228.jpg
    1.3 MB · Views: 1
I also found this in my gold powder when washing it it looks like paper but coated in gold. I'm 99% certain that there was nothing in there when doing this procedure that looks like this. There wasn't anything in there. I have it now sitting in Hcl.
 

Attachments

  • 16644043445961124855768992480599.jpg
    16644043445961124855768992480599.jpg
    1.6 MB · Views: 1
I also found this in my gold powder when washing it it looks like paper but coated in gold. I'm 99% certain that there was nothing in there when doing this procedure that looks like this. There wasn't anything in there. I have it now sitting in Hcl.
Nevermind I tested it and it was simply gold that somehow made a film of sorts. So I just redissolved it. 😁
 