Is there any buyers online for ore? Unknown composition 39.2 pound. Or what do you think is the best route to selling this
 

Attachments

  • PXL_20210901_083656463.jpg
    PXL_20210901_083656463.jpg
    1.9 MB · Views: 121
  • PXL_20210901_083613823.jpg
    PXL_20210901_083613823.jpg
    1.8 MB · Views: 121
  • PXL_20210901_083607798.jpg
    PXL_20210901_083607798.jpg
    2.1 MB · Views: 118
  • PXL_20210901_083602856.jpg
    PXL_20210901_083602856.jpg
    1.8 MB · Views: 117
  • PXL_20210901_083515057.jpg
    PXL_20210901_083515057.jpg
    1.8 MB · Views: 123
Google where to get a fire assay, then after, (if), you know you actually have something worth buying, google where to sell gold bearing ore.
 
That is mica schist with dark red almandine garnets. There seems to be some pyrite too based on the rust. Nice in a garden but I don't see any ore there.

The silvery shining rock is because it is full of fine mica. We got a mountain range full of this type of stone.

Göran
 
That is mica schist with dark red almandine garnets. There seems to be some pyrite too based on the rust. Nice in a garden but I don't see any ore there.

The silvery shining rock is because it is full of fine mica. We got a mountain range full of this type of stone.

Göran
Why are you this much pessimistic? If you are professional, you must see that the stone is wet and there is no shine of mica on them!
 
Why are you this much pessimistic? If you are professional, you must see that the stone is wet and there is no shine of mica on them!
Better to be pessimistic than optimistic, otherwise you'll get let down 9 times out of 10. Especially with stuff like ores. But he's right, that looks like very fine mica.
 
Is there any buyers online for ore? Unknown composition 39.2 pound. Or what do you think is the best route to selling this
if it is of "unknown composition", how you know that it is ore ? :) how you price something unknown ? where it came from ? wich type of rock/geology it belong to ?
from the pictures, it can´t be determined if they arent focused and detailed. from these photos, i have no clue.
i know at least 20 minerals/rock types which looks exactly like this: greyish-brown rock :D bit shiny, bit ugly, bit like every other rock around.
only thing that i could advice is:
ASSAY, ASSAY, ASSAY
 
Why are you this much pessimistic? If you are professional, you must see that the stone is wet and there is no shine of mica on them!
I'm with ya on the negative people. It's like a disease or something... It's on everything I read. Everyone wants to shoot someone down. And most times they are wrong and have no basis for what they say. Other than opinion. Shew! Boy are country is doomed I'm afraid
 
I've got some more myself and a meteorite.. I'd love to get rid of. Did you find a buyer for your mica?
 

Attachments

  • IMG_20220801_232435567.jpg
    IMG_20220801_232435567.jpg
    3.2 MB · Views: 1
  • IMG_20220814_201938508.jpg
    IMG_20220814_201938508.jpg
    1.2 MB · Views: 0
  • IMG_20220814_201931344_1.jpg
    IMG_20220814_201931344_1.jpg
    1.2 MB · Views: 0
  • IMG_20220814_201931013.jpg
    IMG_20220814_201931013.jpg
    1.5 MB · Views: 0
  • IMG_20220801_232358647.jpg
    IMG_20220801_232358647.jpg
    2.7 MB · Views: 0
  • IMG_20220814_201939387_1.jpg
    IMG_20220814_201939387_1.jpg
    1.1 MB · Views: 0
  • IMG_20220801_232529401.jpg
    IMG_20220801_232529401.jpg
    2.9 MB · Views: 0
  • IMG_20220801_232520571.jpg
    IMG_20220801_232520571.jpg
    2.6 MB · Views: 0
FYI, there are realists on this forum, and a lot of talkers who cannot walk the talk.An ore is a mineral compound that can be mined, milled, and sold for a profit. If you cannot do that, it is not ore. It is a mineral of some known composition, maybe containing some PM's, but if it cannot be sold for a profit, it is not ore. The Moderators and professionals here can get frustrated with rookie claims of claiming it has Au in it, and it might, but if you don't know the difference between an ore and an unsalable mineral, but doubt the quality of knowledge on this forum, we have seen this type of behavior several times a week.I have 40 years in the mining, metals industry, and I learn a lot from these guys. One of the best lessons I have learned here is knowing when to shut the F--8* U(, and listen as well as a little humility. Listen to the right people, not the others trying to make friends like this is a Facebook site, or something.We would love to help you, but you have to also help yourself. Don't make false claims based on a feeling. This is a site of the known science of helping others refine Gold, and other precious metals, with associated processes.Before jumping on the so called pessimists for doubting you, please learn to speak our language. I hope you stay with this site long enough to gain some knowledge, and finally see what we are talking about.
 
I've got some more myself and a meteorite.. I'd love to get rid of. Did you find a buyer for your mica?
I’m not very deep into minerals, but I doubt it is a meteorite, it looks more like some kind of iron mineral with oxidised interior or similar.

The rock seem to be of iron compound too. You can see where the water has penetrated and oxidised the iron or dragged iron into the porous rock.

It would be nice if it was a meteorite though😏
 
Koinking99,

Would you pay for a rock because it glitters nicely?
There are a lot of minerals that look fantastic like a unicorn poo but they're good for a mineral collection only, not for getting precious metals out of it.
Judging a mineral by a photo is very difficult.

It's better to be sceptical than freaking out because you think you found a whole mountain of gold and nobody noticed this before you.
Get an proper result about the "rich ore".
If you know for sure, you are rich (not the guy who owns the mine/claim), you can think about quitting your job, leaving your wife, buying a sports car…

btw: Your meteorite could be a concretion.
https://sites.wustl.edu/meteoritesite/items/concretions-3/
 
Koinking99,

Would you pay for a rock because it glitters nicely?
There are a lot of minerals that look fantastic like a unicorn poo but they're good for a mineral collection only, not for getting precious metals out of it.
Judging a mineral by a photo is very difficult.

It's better to be sceptical than freaking out because you think you found a whole mountain of gold and nobody noticed this before you.
Get an proper result about the "rich ore".
If you know for sure, you are rich (not the guy who owns the mine/claim), you can think about quitting your job, leaving your wife, buying a sports car…

btw: Your meteorite could be a concretion.
https://sites.wustl.edu/meteoritesite/items/concretions-3/
Excellent information from BlackLabel.
Thanks mate.
 
No. Your absolutely right about that. Nobody will purchase material of this nature sight unseen. Because hell...let's face it...that's the real fun of it . Pondering on something until it reveals itself as to what it is..But positive is my charge. I do a little buying here and there. If anybody needs to offload some metals. By the wzy
 
Can anyone tell me what this is maybe have about a fifty pound rock of it
 

Attachments

  • 16942754965421360454019017444009.jpg
    16942754965421360454019017444009.jpg
    1.2 MB · Views: 0
Can anyone tell me what this is maybe have about a fifty pound rock of it
Welcome to us.
Is far as I can see, some kind of Gneiss.
And unless you have an assay, it is just a rock anyway.

It is next to impossible to identify minerals/ores/rocks by pictures alone.
Try to crush it fine and pan it, if it has Gold in it it will show itself then.
 