future gold refiner
Active member
Hello,
I want to refine some waste which consists of differend precious metals.
I decided to use a ammonium thiosulfate / ammonium leach with copper as catalyst. (because its harmlessness)
my question: which precious metals are leachable with this leach except for gold and silver?
...platinum ?, palladium ?... other platinum group metals?
thanks a lot for answer.
I want to refine some waste which consists of differend precious metals.
I decided to use a ammonium thiosulfate / ammonium leach with copper as catalyst. (because its harmlessness)
my question: which precious metals are leachable with this leach except for gold and silver?
...platinum ?, palladium ?... other platinum group metals?
thanks a lot for answer.