White crystals in AR bottom?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

gogoldgold

Member
Joined
May 19, 2007
Messages
14
IMG_1115.jpg

IMG_1116.jpg

Put the 20gm 22karat scrap gold in AR test, can not work and leave small white crystals in the bottom.
 
GOGO:

Low temp causes that. No problem, just put it on hot plate and heat up to about 120 to 150 degrees F and it will disolve. then you can neutralize it and drop the gold.

You may want to keep the AR in a warm location to keep this from happening.