Heey guys from Philippines. I got a lot of questions. I badly needed help, suggestions and HEELP. And ADVICE. IM making stupid decisions.
1. When I precipitated Gold in the bucket using SMB, the next day only gray to white precipitate were there and the solution is still green. (Is it because I added too much SMB). Did the gold still remain in the solution?? I saw a YouTube vid showing that it just needed to be washed by HCL during filtration. Then I proceed as the usual, Making AR solution again from the filtration to refine it once again. And precipitated it with SMB. Then proceeded to melting.
2. At the melting process, the sediments were in the filter paper and carefully burned it. Not having any of them flying out. I added a few sparkles of soda ash and more borax. Much Borax it seems, and the result was black substances and less gold.
IN context I processed 600 grams of IC chips, 100 grams of gold-plated fingers and Ribbon flex from HDD. I burned the ribbon flex and IC chips and grinded it. What do you think guys??? I need help and I'm almost going to cry.
1. When I precipitated Gold in the bucket using SMB, the next day only gray to white precipitate were there and the solution is still green. (Is it because I added too much SMB). Did the gold still remain in the solution?? I saw a YouTube vid showing that it just needed to be washed by HCL during filtration. Then I proceed as the usual, Making AR solution again from the filtration to refine it once again. And precipitated it with SMB. Then proceeded to melting.
2. At the melting process, the sediments were in the filter paper and carefully burned it. Not having any of them flying out. I added a few sparkles of soda ash and more borax. Much Borax it seems, and the result was black substances and less gold.
IN context I processed 600 grams of IC chips, 100 grams of gold-plated fingers and Ribbon flex from HDD. I burned the ribbon flex and IC chips and grinded it. What do you think guys??? I need help and I'm almost going to cry.