Hello guys
Merry Christmas’s to all You .
I do an experiment with some Ore and I use a precipitation using a piece of Zinc metal.
and the precipitation turn very brown and coagulate very fast
I never had that kind of Brown color before
and it was way fast.
When i precipitate before ,I always had Black and very dark brown
precipitation .
I will post the pictures so you guys can judge my work .
and can give me any advice.
Thanks
Edited.
I add two pictures of the pan with
the concentrate and i believe it is gold there.
Merry Christmas’s to all You .
I do an experiment with some Ore and I use a precipitation using a piece of Zinc metal.
and the precipitation turn very brown and coagulate very fast
I never had that kind of Brown color before
and it was way fast.
When i precipitate before ,I always had Black and very dark brown
precipitation .
I will post the pictures so you guys can judge my work .
and can give me any advice.
Thanks
Edited.
I add two pictures of the pan with
the concentrate and i believe it is gold there.