A Anonymous Guest Sep 1, 2008 #1 am I correct in assuming that zinc will not drop iron or nickel? thanks, Jim
P Platdigger Well-known member Supporting Member Joined Jul 26, 2007 Messages 1,662 Location Washington Sep 1, 2008 #2 Given the right "ph", zinc should displace anything above it on the electromotive scale.......and that would include iron and nickel. Randy
Given the right "ph", zinc should displace anything above it on the electromotive scale.......and that would include iron and nickel. Randy
A Anonymous Guest Sep 1, 2008 #3 maybe I did not ask the right question, zinc being more active may displace iron and nickel but are they active enough to react with water in the solution to keep them in a non-metallic form?
maybe I did not ask the right question, zinc being more active may displace iron and nickel but are they active enough to react with water in the solution to keep them in a non-metallic form?