All,
This is just a place holder for a post with the complete poor man's AR process.
Poorman's AR Process
Steve
This is just a place holder for a post with the complete poor man's AR process.
Poorman's AR Process
Steve
hoardpm said:Sounds like regular AR is just a little easier to use. Do you have any data on the cost advantage...if any?
Sam, Wash with water, then let settle until the color of the wash water is no longer blue. If you want to be extra clean test a few drops of the rinse water with a drop ammonium hydroxide (3% unscented household ammonia will do), a blue color indicates coper is still present and you should wash some more. After the water rinses hot HCl and water rinses are good.sam said:diluted yesterday (1:2.5 ratio)' i'm gonna wash with water 3x and then HCL 3x
would you recommend hot HCL wash?
See note above about 3% ammonium hydroxide, you should be able to get it in any grocery store. I personally don't wash with nitric any more at all.sam said:i don't have at the moment ammonium hydroxid or nitric acid to add to the washing phase...
Yes, cell powder may contain some silver.sam said:i understand i'm risking having silver in my powder?
Depends on your goal:If you want pure gold then dissolve, filter free of particulate, and precipitate with SMB.sam said:should the powder from the cell be dissolved (HCL+cl) or just wash and melt?
My money says its SO2, but I wonder if it's possible to create hydrogen sulfide by this process? Could prove deadly if you breath much if it is.samuel-a said:BTW, what are the fumes (and terrible smell) that is coming out whan addind the SMB ?