Stannous Chloride – Test For Gold, Platinum and Palladium Presence
Stannous chloride test solution is one of the most important tool and a most have for any precious metal recovery and refining process, this test solution will tell you if there is presence of dissolved precious metals (gold, platinum and palladium) in a solution or not.
On this article we will go over: how to make by your self Stannous Chloride test solution, testing principles and show how test results should look like.
Read More:
Stannous Chloride – Test For Gold, Platinum and Palladium Presence
just relesed a new article at my website:
Stannous Chloride – Test For Gold, Platinum and Palladium Presence
Stannous chloride test solution is one of the most important tool and a most have for any precious metal recovery and refining process, this test solution will tell you if there is presence of dissolved precious metals (gold, platinum and palladium) in a solution or not.
On this article we will go over: how to make by your self Stannous Chloride test solution, testing principles and show how test results should look like.
Read More:
Stannous Chloride – Test For Gold, Platinum and Palladium Presence