mlgdave said:Does anyone know the ratios of acid in the test solutions? Instead of paying 29.00 on ebay I would like to make my own? I imagine its just different formulations of nitric and Hcl?
mlgdave
jimdoc said:Thanks for bumping this thread, The Pawnbrokers Guide to Testing Metals needs to be seen by all newbies.
No thanks on your spam.
Jim
samuel-a said:jimdoc said:Thanks for bumping this thread, The Pawnbrokers Guide to Testing Metals needs to be seen by all newbies.
No thanks on your spam.
Jim
Who? What? Why? and When?
samuel-a said:mlgdave said:Does anyone know the ratios of acid in the test solutions? Instead of paying 29.00 on ebay I would like to make my own? I imagine its just different formulations of nitric and Hcl?
mlgdave
I can't find the post, it's by Harold or GSP (sorry can't remember who)
so I'll just write the ratios:
10K - 22.2ml nitric to 7.4ml distilled water
14K - 23.7ml nitric to 5.9ml distilled water to 10 drops of HCL
18K - 5.9ml nitric to 5.9ml distilled water to 22.2ml HCL
for 22K i just used 1 part nitric to 4 parts HCL
That is working great for me.