Has anyone processed them like this?
Is the gold there good or the same as on the motherboard connectors?
Greetings.Those may be "signal" relays, which jogged my memory, I have 2000+ of these and arthritis in both my thumbs.
Gold-clad silver says the datasheet.
Shame I never run across these Pd ones just whatever kind of Ag ones. But I had better luck with soviet potentiometers and relays0,24 gramm
silver-palladium alloy 80/20.
The middle contact (normally open) is just a solid piece.
everything is silvered on top.
The thickness of the silver plating is visible after the burner.
people knew how to do 50 years ago.
such only until 1977, then simple silver...Shame I never run across these Pd ones just whatever kind of Ag ones. But I had better luck with soviet potentiometers and relays