kelly said:I've found gold in laptop LCD screens. If you look real close or with a magnifying glass you'll see gold wires running around three sides of the board (nec versa s/33 and an old compaq). Fine as a hair, but quite a bit of it. I haven't processed any yet partly due to time and partly because its sealed under some kind of silicone. I'm still in the gathering, learning stage. Thanks to this site and the people on it I feel for the first time that I can actually successfully process the stuff I've hoarded. I've been reading and watching and rereading and rewatching. All I can say is
THANK YOU! This forum and you guys rock!