ilyaz said:
I pulled out these two pieces from an LCD monitor. They are about 12" in length and seem to be gold-plated on one side. At least they have a typical "gold" color on one side and "usual" stainless steel look on the other. So is this gold on the front or not? Thanks.
They are actualy transparent stickers yellowish in color was a heartbreaker finding that out as i had 30 something saved just like it.
 
ilyaz said:
I pulled out these two pieces from an LCD monitor. They are about 12" in length and seem to be gold-plated on one side. At least they have a typical "gold" color on one side and "usual" stainless steel look on the other. So is this gold on the front or not? Thanks.

Aluminum anodized in Golfen color shade...

That typical gold color is not gold...

Thanks
 