misterstink
Member
- Joined
- Dec 11, 2017
- Messages
- 5
Second edit: I just realized that there is an entire forum dedicated to sampling/assaying/testing - Please let me know if this belongs there more than here.
I was testing a mixture of unusually heavy cons in my pan along with a few larger pieces (about 1/3rd the diameter of a copperhead BB). Dissolved it in aqua regia, and the attached = the results roughly a minute after applying about three week old Stannous chloride.
This is a very colorful combination. Fairly certain it tests positive for gold and palladium. Just hoping for some more experienced opinions.
Thanks.
Edit: Adding another picture, from the same ore, treated in the same manner. Was wondering about that somewhat orange/rust/yellow-brown color could be platinum? This photo was taken maybe 30 seconds after.

This is a very colorful combination. Fairly certain it tests positive for gold and palladium. Just hoping for some more experienced opinions.
Thanks.
Edit: Adding another picture, from the same ore, treated in the same manner. Was wondering about that somewhat orange/rust/yellow-brown color could be platinum? This photo was taken maybe 30 seconds after.