M ms32462 Well-known member Joined Jun 22, 2011 Messages 69 Jul 13, 2011 #1 WHAT IS THE PERCENTAGE U SHOULD USE 30% 40% 50% I SEEN LAZERSTEVE VID HE USED 70 % WAS WOUNDERING THE STRONGER THE BETTER OR IS IT BY WHAT U WANT TO USE ????? % WISE THANKS
WHAT IS THE PERCENTAGE U SHOULD USE 30% 40% 50% I SEEN LAZERSTEVE VID HE USED 70 % WAS WOUNDERING THE STRONGER THE BETTER OR IS IT BY WHAT U WANT TO USE ????? % WISE THANKS
M martyn111 Well-known member Joined Dec 18, 2009 Messages 450 Location Stockport UK Jul 13, 2011 #2 Firstly drop the all capitals in your post, it isn't considered polite and chances are you will be ignored. To answer your question, for general purpose use, nitric acid is diluted using distilled water, 70% nitric would be diluted 50/50
Firstly drop the all capitals in your post, it isn't considered polite and chances are you will be ignored. To answer your question, for general purpose use, nitric acid is diluted using distilled water, 70% nitric would be diluted 50/50