Johnduda1
Member
Can anyone tell me how to do the hydrochloric acid test on rocks and does it work to see if there might be valuable minerals in that rock
It is not recommended to add acids to rocks that have not been assayed.Can anyone tell me how to do the hydrochloric acid test on rocks and does it work to see if there might be valuable minerals in that rock
See Quick Qualitative Testing of Rocks and Ore.Can anyone tell me how to do the hydrochloric acid test on rocks and does it work to see if there might be valuable minerals in that rock
No. To see what's in a rock you crush it to fine powder and pan it.Can anyone tell me how to do the hydrochloric acid test on rocks and does it work to see if there might be valuable minerals in that rock
I'm not just looking for gold I'm looking for other valuable minerals and minerals that could be present in rocksNo. To see what's in a rock you crush it to fine powder and pan it.
Or you have it assayed.
If you have specimens that need cleaning, as said, adic is not recommended on unknown rocks.
Here is a video of a you tuber i like to watch.
He tries out different acids and the result of Nitric was not good.
Strong HCl did the best.
Now he does not mention the dangers of things like arsenic, cyanide or mercury in the rocks, but they are all from the same mine. Maybe he knows there is nothing to worry about.
Geology reports of the area where you found it could help.
But if there is no visible gold, i would start with crushing and panning.
No. To see what's in a rock you crush it to fine powder and pan it.
Or you have it assayed.
If you have specimens that need cleaning, as said, adic is not recommended on unknown rocks.
Here is a video of a you tuber i like to watch.
He tries out different acids and the result of Nitric was not good.
Strong HCl did the best.
Now he does not mention the dangers of things like arsenic, cyanide or mercury in the rocks, but they are all from the same mine. Maybe he knows there is nothing to worry about.
Geology reports of the area where you found it could help.
But if there is no visible gold, i would start with crushing and panning.
I'll
I have heard that Carbonite rocks can contain rare earth metals is that trueGeologists typically use dilute HCl to test for carbonate rocks, not for valuable minerals. There are qualitative tests using a few grams of material in a test tube to look for specific reactions. These tests, in conjunction with a bead test, can be accomplished in the field. A handheld XRF has largely replaced these methods in most mid-sized and larger exploration efforts
As far as I know, there are no single simple "acid" test to test a rock for values.I'll thank you for your response is there a simple acid test for silver and rocks
Which rare earth metals?I have heard that Carbonite rocks can contain rare earth metals is that true
Mountain Pass has rare earths in carbonatite (not carbonate) intruded into PC gneiss. In general carbonates are marine sediments.I have heard that Carbonite rocks can contain rare earth metals is that true
Schwerters test.Can anyone tell me is there a simple way to test for the presence of silver using chemicals
If for rocks, the link provided in post #3 on this thread has what you need. If metal alloys, try the previous post, #16 in this thread.Can anyone tell me is there a simple way to test for the presence of silver using chemicals