I've tried couple of blenders. And really didn't have alotvof success in grinding up Motherboard cpu sockets.
But the old sausage grinder does fairly well. It's still a little work involved...but it's better than the blenders I tried to use. I'm gonna grind it again using the medium blade. Any other ideas , please feel free to add your comments. Be Safe.