rocksmashmouth
Member
Thanks to all those who make this forum possible.
Please describe your process.I've been smashing rocks for a year now and have a pretty good tech.for isolating the incapacitated gold from solfide rich ore.
However I haven't melted any of the product or sold any yet ,want to tho.
Where did you find this process ?First thing is obtaining the sulfide rich rock.Once you have that crush said rock untill most of it is beach sand size.Now pan out the material using soap untill water is almost clear.Next combine in a glass container with one part vinegar three parts H2o2 and a table spoon salt for every cup of liquid,it doesn't have to be exact with the salt. stir the mixture.add low heat and wait 48 hours stirring every 3 to 4 hours and adding H2o2 to compensate for evaporation.now add half part acetone stir and wait 12 hours.next rost untill no smoke comes out . return material to the salutation add more vinegar and more H2o2 wait 24 hours and rost again .now float out the ultra fine gold.
Do you know if your rock has Mercury, Arsenic or Cadmium in it?First thing is obtaining the sulfide rich rock.Once you have that crush said rock untill most of it is beach sand size.Now pan out the material using soap untill water is almost clear.Next combine in a glass container with one part vinegar three parts H2o2 and a table spoon salt for every cup of liquid,it doesn't have to be exact with the salt. stir the mixture.add low heat and wait 48 hours stirring every 3 to 4 hours and adding H2o2 to compensate for evaporation.now add half part acetone stir and wait 12 hours.next rost untill no smoke comes out . return material to the salutation add more vinegar and more H2o2 wait 24 hours and rost again .now float out the ultra fine gold.
The best way is roastingTo get rid of sulfides the two best ways are roasting in open air with a fan blowing the liberated sulfur dioxide away from you or slow additions of 30% hydrogen peroxide on low heat going very slow so as not to overflow...very reactive...until there us no more reaction this oxidizes the sulfides. This dies not dissolve any of the base metals etc.
You must after this dry a sample and get it tested. You need to know what you're dealing with before you ever add acid to anything like this or any ore.there can be all kinds of ugly elements that can harm you physically or the environment if not properly handled and that can lock up or steal any precious metal that nay be there. Always test an ore before doing anything so you know what you're dealing with or it can get you killed.
Great advice, but;The best way is roasting
The best way is roasting
Using Hydrogen Peroxide to oxide sulfides will release lot of fumes
that is highly toxic.
too dangerous.
and the amount of waste solution is high.
And have to use lot of Hydrogen peroxide.
the cheapest way is roasting the sulfides in an Iron pan until is glow red.
after that You can panned the roasted sulfide.
some people that I Know crushed the roasted sulfide to be sure that will release all the gold.
if the the sulfide contains gold.
then panned the pulverize roasted sulfide.
I'd guess the majority is SO2.Which fumes are created by H2O2 on sulfides by the way?
My friend don’t put Your words in my mouth.Great advice, but;
You write it as if you have done it many times and consider it completely safe.
Is that also the best way when arsenic, mercury, cyanide, asbestos, and more such unhealthy compounds are present in the ore?
Do the fumes released by roasting need to be cleaned or scrubbed? Are they perhaps toxic and dangerous, even more than H2O2 fumes?
Are there any safety precautions you would like to add to this advice for novice you tube copy cats?
The danger in providing step by step instructions, is that people will follow them without any experience or knowledge.
Have you filled in all the possible side track scenario's and what to do to prevent an accident or control the effects once occurring?
Be prepared to get sued. The parents of one particularly 'smart' kid can find your given instructions that led to his death and send a lawyer your way.
And please don't say: "i expect people to have a certain level of experience, you don't fly to the moon without training.... "
there are a lot of people who don't think enough or at all.
I've noticed this writing style in your messages a couple times now and decided to point this out. Write disclaimers or don't write instructions, is my advice.
I think we have a language barrier here. I was referring to the roasting if you have done it before and what fumes are emitted during this process.My friend
Maybe You confuse what i was posting
i post the dangerous of using that chemical.
I’m a miner
My knowledge of chemistry is very limited .
i will do my best in advice ,base in my knowledge.
Yes i did it before
and it was a huge mistake.
Using Hydrogen peroxide to oxide sulfides is Not safe at all.
it will release very nasty and dangerous fumes,very dangerous to your health.
and is Not economical at all.
the amount of Hydrogen Peroxide use it to oxide sulfides is huge.
then You have to deal with the waste solution that is huge
so the return is Nothing, compare with the amount of money You will need to spend i buying the chemical and get rid of the waste solution.
i advice every one Not to do it.
is Not safe at all and it will kill You.
SO2 can poisoning Your and stay in Your body for a long length of time
and do the damage in Your body slowly .
SO2 (above 1 ppm) results in increased incidence of pulmonary symptoms and disease, decreased pulmonary function, and increased risk of mortality
No minors allowed on the forum, but YES miners allowed in the forum?My friend i forgot to write that i will fix it.
ty for remind me that.
This refining forum should be for adult only
18+
No minors should be allows in the forum
that’s one thing to be consider
and put it very clear in the forum
only for adults.
Because refining and mining is Not
for minors
we dealing with many chemicals and No minor should be allows in the forum.
by posting that in the forum page
as a disclaimer
will save any member for any legal thing.
because any one can twisted any post
in their lack of knowledge and use it
in their own opinion.
and as they please it and get hurt by their own stupidity .
Enter your email address to join: