Has anyone experience with rhenium reclamation from solution?
I've got solution containing approx. 1-2g/litre of rhenium as rhenium nitrate and possibly perrhenic acid, and am wondering, whether it would be worth the effort to reclaim rhenium from the solution(as i currently have no idea how to
)
Also, Has anyone practical experince as what does hydrochloric acid do with 30Cu30Sn40Pb alloy? My guess is that it should slowly eat away Pb and Sn, leaving Cu sponge behind. Can someone confirm or refute?
Thanks for any advice
Best Regards
Has anyone experience with rhenium reclamation from solution?
I've got solution containing approx. 1-2g/litre of rhenium as rhenium nitrate and possibly perrhenic acid, and am wondering, whether it would be worth the effort to reclaim rhenium from the solution(as i currently have no idea how to
Also, Has anyone practical experince as what does hydrochloric acid do with 30Cu30Sn40Pb alloy? My guess is that it should slowly eat away Pb and Sn, leaving Cu sponge behind. Can someone confirm or refute?
Thanks for any advice
Best Regards