• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

AP on my way

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
I think this still belongs in this thread:I'm letting you know that I restarted a batch today. I used the liquid that was left over from yesterday, added some acid and some persulfate. I didn't measure anything. ERROR! Instead of 6 hours, the biting continues now, so 8+ hours.
 
If the time spent is small, then it certainly outweighs the consumption.
I guess that depends how you look at it- and how you organize it. Certainly the time from start to finish is shorter, but the proportion of time you have to actively work with it could be much higher.

Part of the charm of our classic style Copper Chloride etching is the comparatively passive nature of the process. It takes a few minutes to set the etch going, and maybe an hour or so at the end to recover the foils, the time inbetween doesn't require continuous monitoring so for me it doesn't count quite the same.

I like to have multiple etches running concurrently at different stages, so I nearly always have something to do and some foils ready to recover, and I can fit it around my other activities easily without committing large chunks of time.

The idea of turbo-etching is very attractive, but realistically my process works out pretty well for me at a relaxed pace. It's a luxury hobbyists can afford which commercial refiners may not.
 
I like to have multiple etches running concurrently at different stages, so I nearly always have something to do and some foils ready to recover, and I can fit it around my other activities easily without committing large chunks of time.
This then requires more containers, more heating plates, more space...Unfortunately, I don't have all of that. I don't have the time either, my days are numbered - I have liposarcoma in my abdominal cavity.
 
This then requires more containers, more heating plates, more space...Unfortunately, I don't have all of that. I don't have the time either, my days are numbered - I have liposarcoma in my abdominal cavity.
I am sorry to hear that.

But to create a productive system does not necessarily mean a lot of extra space or equipment. My workspace is a 1mx1m wooden box, containing about a dozen 5L recycled water bottles. I don't use extra heating, I have a single bubbler which I move between the bottles as needed. I recover foils by filtering, and start new etches at the same rate, so there is a constant stream of material passing through. Although each etch may take a week or two, effectively I am putting new material in and taking foils out on the same day, if you see what I mean, and my commitment of actual working time is minimal as I don't need to be present for most of the reaction time.

I'm still very impressed with the new method you have shared, but on consideration I don't think it's appropriate for my work pattern at the moment. You are right though, if I were working at a larger scale, then speed would be more critical and/or the space needed would be larger.
 
This then requires more containers, more heating plates, more space...Unfortunately, I don't have all of that. I don't have the time either, my days are numbered - I have liposarcoma in my abdominal cavity.
Too bad, I wish you the best in the time to come.

You really do not need anything advanced, plastic buckets will do.
If you have many in different stages it don't matter much that it takes time, there will always be one that is almost ready..
Just make sure you have someone well informed that can help to clean up, if things go too fast downhill.
 
A large air pump with a gang valve from an aquarium can be used to provide air to multiple solutions at a time. The pump I had would run enough air to keep 8-10 five gallon buckets of AP working steadily. It could also keep 3-4 fifty gallon drums working. I don't recall the brand but they are used in large aquariums like those used for raising talpia. 10 years ago I paid around $250 for the large pump, I don't recall on the valve price. I will say I ran very few pins in them as I made anode bars from the pins for a copper cell.
 
I was really worried about my gold. I had to check the gold content in the solution using white paper. Here are the results.
The white paper before I soaked it in the solution.IMG_20250304_133517.jpgIMG_20250304_133628.jpg
■ The white paper before I soaked it in the solution.
■ The paper soaked in the solution.
■ The paper after I added two drops of CuSn.
I'm sure there was no gold in the solution, which would be of some value.


P.s.: How do I add text exactly under a specific photo?
 
Last edited:
I was really worried about my gold. I had to check the gold content in the solution using white paper. Here are the results.
View attachment 67341View attachment 67342View attachment 67343
■ The white paper before I soaked it in the solution.
■ The paper soaked in the solution.
■ The paper after I added two drops of CuSn.
I'm sure there was gold in the solution, which would be of some value.


P.s.: How do I add text exactly under a specific photo?
Use a cotton bud or a strip of white paper one cm wide and appr 5 cm long.
Dip the tip of the cotton bud into the solution and add one drop of Stannous on the upper part of the cotton part.
Or dip the tip of the paper into the solution, then drip one drop of Stannous next to the wet part of the paper and observe as they come together.

I can see no evidence of Gold here, it may be the lighting and photo quality though.
 

Latest posts

Back
Top