2 oz 10k shot in HCL and SubZero 2:1
I had a batch going on low heat and was called away for emergency 8 hrs later my batch is almost dried out with sediment.
What can I add to get more liquid to work with to filter before dropping?
I'd still be tempted to add water first it's cheaper and then add a little Hcl you might also have to add some more of your nitrate to complete your dissolution.